FAQ

Frequently asked questions about adhesives

Answers to the questions our customers ask most often — product selection, application, curing, packaging and storage, and technical support.

Selection & Matching

Can your products replace the imported grade we currently use?

We can match by application and performance, but not item-for-item equivalence. We need the current product data sheet plus failure details: where the joint failed, service time, temperature and media. We then propose an equivalent grade and explain the main differences.

Strength, working time, temperature resistance and gap filling often differ. Confirm those differences before switching, and do not change over a production line without validation.

What should I specify in advance when bonding two different materials?

Describe both substrates and their surface condition: whether they are plated or coated, whether there is an oil film, and whether they are recycled materials.

Metal-to-plastic and metal-to-rubber combinations require different adhesive chemistries. Low-surface-energy plastics usually need pre-treatment or a dedicated grade; joints with a large thermal expansion mismatch should use a tough, lower-modulus adhesive, because hard and brittle bond lines tend to crack under thermal cycling.

What if the application is complex and I am not confident about the choice?

Give us the joint location, substrates, temperature range, contact media, loading mode and current failure symptoms. We will recommend a grade and alternative approach based on that information.

For complex applications, validate with the smallest available sample pack before moving to volume production.

There are so many models—how do I choose the right one?

Narrow the range down with three questions: what materials are being bonded or repaired, what problem you need to solve (reinforcement, leak sealing, threadlocking or sealing), and what temperature and media the joint will see. First rule out any model whose substrate is not on the approved list, then compare cure speed, gap-filling capability and temperature margin.

This step only establishes direction. Final confirmation should come from a trial: run a control sample on the same joint and record cure time, strength and appearance—more reliable than a data sheet alone.

How do I choose within the instant adhesive range? What is the difference between 401, 402, 403 and the low-viscosity grades?

For general bonding, choose 401; for high temperature or near heat-generating components, choose 402; for appearance parts, transparent parts and low-odor requirements, choose 403 or 460; for penetrating tiny gaps in assembled parts, choose low-viscosity grades such as 406 or B495/B496.

Where impact resistance, peel resistance or small-gap filling is needed, prefer the toughened B480. First establish direction by substrate and operating conditions, then confirm cure speed and strength with actual test parts.

How do I choose a threadlocker by strength, and where are 222, 243 and 263 used?

For small screws that are frequently adjusted or serviced, choose low-strength B222, removable with hand tools; for general machinery assembly, choose medium-strength B243; for heavy-duty joints that are rarely disassembled, choose high-strength B263.

For high-temperature applications choose B272; for bolts above M25 choose B277; for reinforcing already-assembled bolts choose penetrating grade B290. The higher the strength, the more disassembly depends on heat or special tools.

How do I select a retaining compound by shaft-to-hub clearance?

For small clearances and fast press fits, choose low-viscosity B609; for general shaft-to-hub fits, choose B603; for worn or oversized clearances, choose B680 with greater gap-filling capability.

For assemblies requiring periodic maintenance or disassembly, choose B641; for high-temperature or oily environments, prefer B620, B638 and B648 respectively. Measure actual clearance and coaxiality before selection.

How do I choose between G168 epoxy AB adhesive and G166 red/blue acrylic adhesive?

G168 is a clear epoxy system with temperature resistance, low odor and high strength, suitable for structural bonding of metals, ceramics, glass and rigid plastics. G166 is a modified acrylic system that cures quickly with good toughness, suitable for fast assembly of magnets, metals and plastics.

Choose G168 for longer working time and higher temperature resistance; choose G166 for fast fixturing and impact resistance. Neither system should replace a production-line adhesive without trial validation.

How do I choose a UV adhesive, and what is the difference between U321, U322 and U323?

Choose U321 for glass, crystal and handicrafts; U322 for transparent plastics such as acrylic, PC and PS; U323 for glass-to-metal and hardware composite parts.

Confirm that the substrate transmits UV light, and check bond-line thickness and lamp distance. If the metal side is opaque, use a dual-cure system or irradiate from the transparent side after dispensing.

For flange sealing, should I choose anaerobic or silicone?

For rigid flanges requiring immediate pressure resistance and high temperature performance, prefer anaerobic types such as G510 and G515; for stamped sheet metal, uneven gaps or slightly distorted flanges, choose semi-flexible G518.

For high temperature or a wider temperature range, choose silicone types G596 and G598; for oil contact, prefer G5699; to replace conventional gaskets, choose G587.

What materials is 401 suitable for bonding?

A general-purpose instant adhesive for fast fixturing of metals, plastics, rubber and wood at small-to-medium gaps, commonly used for fixing small parts on assembly lines.

Porous materials or acidic surfaces slow curing significantly; use a primer and clamp promptly after dispensing to avoid prolonged exposure.

What applications suit the temperature performance of 402?

A high-temperature instant adhesive for joints near heat-generating components, close to electronic soldering, or in higher ambient temperatures.

Long-term temperature should stay within the grade's upper limit; for continuous high temperature, consider a structural adhesive with higher heat resistance.

What products is 403, with low blooming and low odor, suited to?

It suits appearance parts, transparent parts, cosmetic packaging and optical components—applications sensitive to blooming and odor.

Maintain ventilation and control the amount applied; excess adhesive can still cause surface hazing. Avoid wiping the bond line immediately after assembly.

How should 406 very-low-viscosity instant adhesive be used?

Its very low viscosity makes it ideal for capillary penetration into tiny gaps in assembled parts, as well as for fast fixturing of small areas.

After dispensing, prevent adhesive from running onto non-bonded surfaces; on vertical surfaces, control the amount and have absorbent material ready.

Is 460 suitable for assemblies with high appearance requirements?

Its low-blooming, low-odor formula suits appearance parts in plastic and metal, with medium cure speed and good versatility.

Choose between 460 and 403 based on actual blooming and odor requirements; run an appearance comparison before volume production.

What bonding is the toughened B480 suitable for?

A toughened black instant adhesive with good impact and peel resistance, suitable for structural fixturing and small-gap filling between metals, plastics and rubber.

The black bond line reduces visibility, but adhesive volume still needs control; for large gaps, use a gap-filling product or structural adhesive.

What applications suit B495 low-viscosity general-purpose adhesive?

A low-viscosity general-purpose instant adhesive for fast bonding of small gaps and small areas, commonly used in production-line dispensing.

Curing slows when assembly gaps are too large; control fit accuracy or switch to a higher-viscosity grade.

How do I choose between B496 and B495?

B496 is also a low-viscosity general-purpose grade for fast fixturing of plastics, metals and rubber, with a quick fixturing speed.

The main differences are cure speed and substrate feel; choose based on line takt time and trial results.

Where is low-strength removable B222 used?

For small screws, dowel pins and adjusting bolts that need frequent adjustment or maintenance.

Its low strength is not suitable for heavy loads or high anti-loosening requirements; it can be removed with hand tools after assembly.

What connections suit medium-strength B243 threadlocker?

For anti-loosening and sealing of general machinery bolts such as pump bodies, gearboxes and motor end covers.

It can be removed with standard tools; for reassembly, clean off residual adhesive and reapply.

How is high-strength permanent B263 disassembled?

For heavy-duty bolts and critical joints that are rarely disassembled, with strong anti-loosening performance.

Heat to about 250°C and work while hot; forcing the bolt may damage the threads.

What equipment suits high-temperature B272?

For threadlocking and sealing of high-temperature locations such as engines, exhaust systems and hot-oil lines.

Long-term operating temperature should remain below the data-sheet limit; if exceeded, use mechanical locking or a higher-temperature product.

How should adhesive be applied to large B277 bolts?

For bolts above M25, apply adhesive over the full engagement length rather than only at the end.

Large bolts require high tightening torque; confirm the adhesive film has not been scraped off before assembly, and tighten to specification.

How is penetrating B290 used on already-assembled bolts?

It wicks directly into the threads of assembled joints to reinforce anti-loosening or suppress leakage.

Wipe off excess adhesive after application to avoid contaminating surrounding areas. Performance depends on gap and cleanliness; clean heavily oily parts first.

What shaft-to-hub fits suit B603?

A general-purpose retaining compound for conventional retention of bearings, bushings, gears and shafts.

Measure clearance before assembly, and rotate while pressing in to ensure an even adhesive layer.

How is low-viscosity press-fit B609 applied?

For small-clearance, fast press-fit shaft-to-hub structures; its good flow makes rapid assembly easy.

Match press-fit speed to the adhesive working time to prevent it being displaced prematurely.

What temperatures suit high-temperature B620 retaining compound?

For shaft-to-hub retention in high-temperature conditions, such as bearings and bushings near heat sources.

Leave margin in long-term temperature; if exceeded, consider a structural adhesive with higher heat resistance.

What should I watch out for with oil-tolerant B638?

It tolerates light oil contamination, making it suitable for shaft-to-hub fits that cannot be fully degreased in maintenance situations.

Degrease as thoroughly as possible; heavy oil contamination significantly reduces final strength.

What maintenance points suit removable B641?

For shaft-to-hub fits that require periodic disassembly, such as frequently serviced pump shafts, rollers and bushings.

Use special tools or moderate heat during disassembly, and avoid hammering that damages the mating surfaces.

What environments suit high-temperature, oil-tolerant B648?

For shaft-to-hub retention in engines, gearboxes and other locations exposed to both high temperature and oil.

Clean mating surfaces before assembly; an excessively thick oil film reduces strength.

How is B680 used for large-gap repair?

Its strong gap-filling capability suits repair of worn or out-of-tolerance shaft-to-hub fits, reducing the need for sleeving.

For very large gaps, still evaluate coaxiality and load requirements, and use mechanical reinforcement where necessary.

What substrates suit G168 clear epoxy AB adhesive?

For structural bonding and potting of metals, ceramics, glass and rigid plastics; it cures clear with low odor and good temperature resistance.

Mix thoroughly at 1:1 and allow 24 hours at room temperature for full cure; for high-temperature, high-humidity environments, run reliability validation first.

What applications suit G166 modified acrylic AB adhesive?

Fast curing and tough, it suits rapid structural assembly of magnets, metals and plastics.

Odor is relatively noticeable, so work in a ventilated area; for large gaps, apply in layers or use with filler.

Is U321 suitable for bonding glass and crystal?

Highly transparent and non-yellowing, it suits glass furniture, crystal crafts and transparent decorative parts.

Ensure UV light reaches the bond line, and set exposure time and distance according to the process.

What should I watch out for when bonding transparent plastics with U322?

For transparent plastics such as acrylic, PC and PS; it cures quickly and leaves a clear bond line.

Materials such as PC carry a stress-cracking risk; run a small trial and avoid leaving adhesive in stressed areas for extended periods.

Is U323 suitable for glass-to-metal composite parts?

For composite bonding of lighting, hardware and glass, combining a clear appearance with adhesion to metal.

If the metal side is opaque, ensure the transparent side allows UV light to reach the bond line, or use a dual-cure system.

What flanges suit G510 high-temperature formed-in-place sealant?

For formed-in-place sealing of rigid flanges, pump bodies and high-temperature applications, forming an immediate seal.

Apply a continuous closed bead and tighten to specification to avoid interruptions in the seal line.

How is G515 flange sealant used?

For flat-face sealing of rigid flanges such as reducers and pump bodies, replacing conventional gaskets.

Remove old gasket and oil before application, and tighten bolts in stages in a diagonal sequence.

What structures suit semi-flexible G518 sealant?

Its semi-flexible formula suits stamped sheet-metal flanges or joints with slight distortion that need vibration absorption.

Increase the amount moderately for larger gaps, but keep the bead continuous.

What pipe thread sealing suits G577?

For thread sealing of metal pipe fittings, covering common media such as water, gas and oil.

Threads must be clean and dry; apply adhesive over the engagement length, tighten, allow to cure, and then pressurize.

How is one-component G565 pipe thread sealant applied?

For thread sealing of hydraulic and pneumatic lines; the one-component format is easy to use.

Tighten to specification after application, avoiding over-tightening that squeezes out the sealant; do not pressurize before curing.

Can G587 silicone gasket sealant replace a gasket?

In many cases it can replace conventional pre-cut gaskets, and it suits irregular flange faces and sealing points requiring heat resistance.

Apply as a closed bead; confirm the surface is free of oil and old sealant before assembly.

What locations suit high-temperature G596 silicone rubber?

A one-component high-temperature silicone rubber for sealing exhaust systems, high-temperature flanges and heating equipment.

Curing depends on moisture in the air; low temperature and low humidity extend the cure time.

How do I choose high-performance G598 silicone flat sealant?

For metal flat-face sealing with oil resistance, temperature resistance and good flexibility, accommodating thermal expansion and contraction.

Apply a continuous, even bead and tighten according to the torque sequence after assembly.

What media suit oil-resistant G5699 flat sealant?

For flat sealing points that are in long-term contact with oil, such as gearboxes and oil pans.

Degrease thoroughly before use and remove all old sealant; otherwise adhesion and seal life are compromised.

Surface Preparation & Application

How far should surface preparation go?

Remove oil, rust, oxide and dust, then abrade as required by the grade. Oil films, mold release agents and machining fluid residues are the most common causes of failure. After solvent wiping, let the solvent flash off completely before applying adhesive; residual solvent weakens the interface.

After abrading porous parts such as cast iron or cast aluminum, blow out residual sand and graphite dust. For galvanized or chrome-plated parts, check coating adhesion first; if the coating is flaking, treat the base metal before bonding.

How do I measure and mix two-part adhesives?

Dispense by weight or volume—never estimate by eye. When the two components differ in color, mix until the color is uniform and no streaks remain when scraped up; the edges and bottom of the container are easy to miss.

For larger batches, mix in smaller portions. A large single batch can react and generate heat prematurely in the container. Use the mixed adhesive within its working time, and never thin a thickened mix with fresh material.

How long is the working time, and how should I schedule the job?

Working time varies by grade and changes significantly with temperature—it shortens quickly as temperature rises. Schedule summer and winter workshop conditions separately.

Plan backward from surface preparation → mixing → application or potting → curing → load-bearing, and allow the full cure cycle rather than scheduling to the shortest quoted time.

How does gap size affect product selection and application?

For very small gaps, choose a low-viscosity grade that penetrates by capillary action. For larger gaps, choose a filled or thixotropic grade; do not pour too thickly at once—apply in layers to reduce entrapped air.

If the gap exceeds the grade's gap-filling capability, reinforce the structure first (welding, sleeving, mechanical fastening) and then bond. Do not rely on adhesive alone to fill large gaps.

What should I watch out for when working at low temperatures?

Lower temperatures extend cure time. Below 5°C, most grades should not be applied under standard room-temperature conditions, and epoxies are particularly affected.

Bring both the parts and the adhesive to the application temperature beforehand, and heat locally and evenly—never with an open flame. For long-term low-temperature work, tell us in advance so we can recommend a suitable process and insulation method for the grade.

How should surfaces be prepared before instant adhesive bonding, and how much adhesive should be applied?

Surfaces must be dry, free of oil, mold release and dust. Metal parts can be wiped with solvent and allowed to flash off completely; low-surface-energy plastics need a primer, otherwise false bonding is likely.

Apply a thin, even bead—enough to form a continuous film after clamping. Excess adhesive slows curing and increases blooming and squeeze-out. Seal porous materials before applying adhesive.

How should threads be prepared before applying threadlocker?

Threads should be degreased, derusted and dry. For blind holes, control the amount of adhesive so it is not forced to the bottom and trapped as a hydraulic lock; for through holes, apply adhesive around the full circumference of the external thread.

Apply adhesive to the engagement area, not the bolt tip, and tighten to torque specification after assembly. Do not let adhesive enter bearings, oil passages or moving joints.

What should I pay attention to when applying retaining compound?

Degrease and derust both shaft and bore, and keep them dry. Apply adhesive evenly around the circumference of the mating surface, and rotate while pressing in to distribute the adhesive and expel air.

Use enough adhesive that a small bead squeezes out at the joint edge after assembly. Keep adhesive out of bearing races, oil holes and other moving parts, and let the assembly cure undisturbed per the process.

What should I watch out for when mixing AB adhesive?

Dispense according to the stated ratio—do not estimate by eye. Scrape the bottom and edges of the container while mixing until the color is completely uniform with no streaks, avoiding uncured pockets.

Mix only as much as you can use within the working time; a large batch generates heat and shortens pot life. Never thin a thickened mix with fresh adhesive.

What conditions must be controlled when applying UV adhesive?

Substrates must be clean and dry, and the bond line should not be too thick, as this affects through-cure. Set lamp distance, power and time according to the process; moving the lamp slightly during exposure reduces shadowed areas.

For stress-sensitive plastics such as PC, be aware of stress-cracking risk from the adhesive; confirm with a small trial first.

How should flange surfaces be prepared before applying sealant?

Degrease, derust and remove old sealant and burrs from the flange face, and keep it dry. Apply a continuous closed bead, keeping clear of the inside of bolt holes and leaving bolt passages open.

After assembly, tighten in stages in a diagonal sequence to the specified torque, avoiding squeezing the sealant out on one side and creating an interruption in the seal.

Curing, Performance & Rework

How long does it take to cure, and when can the joint take load?

Surface dry, initial set and load-bearing strength are three different points, each listed in the data sheet. Load-bearing strength usually requires full cure; loading too early can damage the bond interface.

Where early handling strength is needed, choose a fast-curing grade or heat-cure. Control heating temperature and ramp rate according to the data sheet—heating too quickly induces internal stress in the bond line.

I followed the instructions but the adhesive did not cure. Why?

Common causes are incorrect mix ratio, poor mixing, oil or mold release on the surface, and low ambient temperature. For anaerobic products, also confirm that the bond line is isolated from air: an oversized gap or insufficient adhesive will prevent curing.

Check these items in order. If the surface is contaminated, extending the waiting time will not help.

Can I drill, tap or machine the cured adhesive?

Repair grades can be machined after full cure. Allow the full cure time, keep tooling sharp, reduce feed rate and use coolant to avoid localized overheating that damages the bond line.

After machining load-bearing areas, recheck for crack propagation and perform non-destructive testing if necessary.

What temperature can it withstand, and will strength drop with long-term heat exposure?

Each grade has a temperature range; short-term peak and long-term service temperatures are different. Running close to the upper limit for long periods accelerates aging and strength gradually declines.

For long-term design, stay within about 80% of the upper limit. Use actual test data and batch records as the final reference; if the range is exceeded, change the grade or the joint design rather than simply adding more adhesive.

The assembly has to be taken apart later—how do I disassemble it?

It depends on strength level: low-strength threadlockers can be removed at room temperature, medium-strength grades rely on tool torque, and high-strength grades must be heated to the specified temperature before removal, following the process document.

For structural bonds, use heat together with wedge separation—safer than impact or prying and less likely to damage the parts. After disassembly, remove all residual adhesive before reassembly; applying new adhesive over old residue creates an unreliable second interface.

How long does instant adhesive take to cure, and how do I separate a misaligned bond?

Fixturing usually takes seconds to tens of seconds, while final strength requires about 24 hours. Low temperature, large gaps or excess adhesive significantly slow the process.

To separate the parts, use a dedicated debonder or acetone allowed to wick along the bond line. Heat accelerates breakdown but may affect appearance parts. After separation, remove all residue before re-bonding.

How long does threadlocker take to cure, and how is it disassembled?

Anaerobic adhesives cure when isolated from air and in contact with metal. Initial set typically takes 10–30 minutes and final strength about 24 hours; low temperatures extend these times.

Low- and medium-strength joints can be disassembled with tools. For high-strength joints, heat to about 250°C and disassemble while hot to avoid twisting off the bolt.

How do retaining compounds perform in terms of temperature and oil resistance?

Standard grades suit general conditions; for long-term high temperature choose B620 or B648; for contact with oil or light oil contamination choose B638 or B648. Refer to the grade data sheet and actual testing for specific temperature ranges.

If the temperature limit is exceeded, switch to a structural adhesive or mechanical reinforcement—do not try to solve it by adding more adhesive.

What are the cure time and temperature performance of AB adhesives?

At room temperature, initial set typically takes 30–60 minutes and final strength about 24 hours; low temperatures extend these times considerably. If early load-bearing is needed, heat curing can be used, but the ramp rate must be controlled.

Leave margin in long-term service temperature and avoid running close to the upper limit. For high-temperature applications, perform heat-aging validation before volume use.

Can UV adhesive cure in areas that light cannot reach?

A pure UV system requires UV exposure to cure; shadowed areas and opaque laminates cannot cure fully.

For such structures, use a dual-cure system, irradiate from a transparent side, or use a primer for local treatment.

Are sealants resistant to temperature and oil, and how are they disassembled?

Anaerobic types suit medium-to-high temperature sealing of rigid structures, while silicone types cover a wider temperature range and remain flexible. For oil contact, select an oil-resistant grade based on the media. Refer to the data sheet for specific temperatures.

To disassemble, separate the flange first, then remove residual sealant with a scraper or dedicated cleaner without scratching the sealing face; leftover sealant will impair the next seal.

Packaging, Storage & Delivery

What is the shelf life, and what should I do with leftover product after opening?

Unopened product has the stated storage life from the production batch date. After opening, keep containers sealed, away from light and moisture. Store two-part A and B components separately, use clean dispensing tools, and never return excess material to the container.

For product beyond its shelf life, first check a small sample for condition and cure behavior before deciding whether it can still be used.

What are the storage requirements, and can low temperatures affect performance?

Store in a cool, dry place away from sunlight and heat—typically 5–35°C; refer to each grade's data sheet for specifics. Storage near heat sources or prolonged high temperatures shortens the usable life.

Some grades thicken or freeze at low temperatures. Let frozen adhesive warm slowly to room temperature and mix thoroughly, then confirm it is normal before use.

What package sizes are available, and can I try a small quantity first?

Common formats are syringes/tubes, bottles, cans and cartridges; sizes vary by grade. The website lists standard pack sizes; special sizes can be confirmed separately.

Samples are supplied in the smallest pack. Volume orders are scheduled by grade and quantity. Tell us in advance if you need repacking, matched kits or custom labels.

How long does it take from order to shipment?

Standard grades ship from stock; non-standard grades and large volumes follow the production schedule, and the lead time confirmed on the order is final.

For urgent orders, state the application and required arrival date. We will first confirm whether the order can be inserted into the schedule or partially shipped in advance; we do not promise what we cannot confirm.

Documents, Samples & Technical Support

How can I obtain technical data and test reports?

Standard parameters are listed on each product page. For more complete written data or batch records, contact us with the grade reference; final values are based on actual testing and batch records.

Third-party test reports are arranged per project and are not readily available for every grade. If you have a specific requirement, tell us early so documentation does not delay your schedule.

I would like to validate a sample first—what is the process?

Describe the application, substrates, operating conditions and what you want to verify. We will send the smallest pack of the recommended grade with application notes.

During validation, run a control group with your current product and record cure time, strength, appearance and failure mode. Send us the results so we can determine whether to change the grade or adjust the process.

Can you send someone on site if we have application problems?

Start with remote troubleshooting: provide photos of the failed parts, application records, mix ratio and ambient temperature. Most issues can be identified at this stage.

For batch issues, process qualification or new line start-up, we can arrange an engineer visit. Time, scope and site conditions must be agreed in advance. Please prepare process records and batch numbers before the visit.

How do you ensure consistency between batches?

We charge raw materials by formula, retain batch samples and perform factory inspection, recording key indicators batch by batch.

For lines sensitive to color, viscosity or cure time, inspection data can be supplied per batch by agreement. If an issue occurs, provide the batch number so we can trace the charging and retained-sample records.

Didn't find your answer? Ask our engineers

Tell us your substrate, application conditions and performance requirements, and we will provide selection advice, sample dispatch and technical support within 48 hours.

×